性能项目 |
试验条件[状态] |
测试方法 |
测试数据 |
数据单位 |
物理性能 |
密度 |
|
ASTMD1505 |
0.907 |
g/cm³ |
物理性能 |
熔流率(熔体流动速率)(230°C/2.16kg) |
|
ASTMD1238 |
8.0 |
g/10min |
机械性能 |
FlexuralModulus-1%Secant2,3(InjectionMolded) |
|
ASTMD790 |
1550 |
MPa |
薄膜 |
SecantModulus-1%Secant,MD4(32µm) |
|
ASTMD882 |
689 |
MPa |
薄膜 |
SecantModulus-1%Secant,TD4(32µm) |
|
ASTMD882 |
689 |
MPa |
薄膜 |
TensileStrength-MD4(Break,32µm) |
|
ASTMD882 |
55.2 |
MPa |
薄膜 |
TensileStrength-TD4(Break,32µm) |
|
ASTMD882 |
37.9 |
MPa |
薄膜 |
TensileElongation-MD4(Break,32µm) |
|
ASTMD882 |
500 |
% |
薄膜 |
TensileElongation-TD4(Break,32µm) |
|
ASTMD882 |
550 |
% |
薄膜 |
ElmendorfTearStrength-MD4(32µm) |
|
ASTMD1922 |
40 |
g |
薄膜 |
ElmendorfTearStrength-TD4(32µm) |
|
ASTMD1922 |
40 |
g |
薄膜 |
SpencerImpact4(31.8µm) |
|
ASTMD3420 |
400 |
g |
光学性能 |
Gloss4(45°,31.8µm) |
|
ASTMD2457 |
85 |
|
光学性能 |
Haze4(31.8µm) |
|
ASTMD1003 |
2.0 |
% |