性能项目 |
试验条件[状态] |
测试方法 |
测试数据 |
数据单位 |
物理性能 |
比重 |
|
ASTMD792 |
0.930 |
g/cm³ |
物理性能 |
表观密度2 |
|
ASTMD1895 |
0.56 |
g/cm³ |
物理性能 |
熔流率(熔体流动速率)(190°C/2.16kg) |
|
ASTMD1238 |
6.8 |
g/10min |
物理性能 |
EnvironmentalStress-CrackingResistance(100%Igepal,RotationalMolded,F50) |
|
ASTMD1693B |
1000 |
hr |
机械性能 |
TensileStrength(Yield,RotationalMolded) |
|
ASTMD638 |
16.9 |
MPa |
机械性能 |
TensileElongation(Break,RotationalMolded) |
|
ASTMD638 |
550 |
% |
机械性能 |
FlexuralModulus-Tangent(RotationalMolded) |
|
ASTMD790 |
552 |
MPa |
可燃性 |
UL阻燃等级 |
1.5mm |
UL94 |
HB |
|
可燃性 |
UL阻燃等级 |
3.0mm |
UL94 |
HB |
|
ADDITIONAL INFORMATION |
补充信息 |
|
TestMethod |
NominalValue |
Unit |
ADDITIONAL INFORMATION |
Pourability2 |
|
ASTMD1895 |
30.0 |
sec |